Effect of Al, Ga, and In Doping on the Optical, Structural, and Electric Properties of ZnO Thin Films
![Thumbnail](/xmlui/bitstream/handle/10234/196556/78621.pdf.jpg?sequence=4&isAllowed=y)
Visualitza/
Impacte
![Google Scholar](/xmlui/themes/Mirage2/images/uji/logo_google.png)
![Microsoft Academico](/xmlui/themes/Mirage2/images/uji/logo_microsoft.png)
Metadades
Mostra el registre complet de l'elementcomunitat-uji-handle:10234/9
comunitat-uji-handle2:10234/7053
comunitat-uji-handle3:10234/8639
comunitat-uji-handle4:
INVESTIGACIONMetadades
Títol
Effect of Al, Ga, and In Doping on the Optical, Structural, and Electric Properties of ZnO Thin FilmsAutoria
Data de publicació
2021-11-01Editor
MDPIISSN
2076-3417Cita bibliogràfica
Porcar, S.; González, J.; Fraga, D.; Stoyanova Lyubenova, T.; Soraca, G.; Carda, J.B. Effect of Al, Ga, and In Doping on the Optical, Structural, and Electric Properties of ZnO Thin Films. Appl. Sci. 2021, 11, 10122. https://doi.org/10.3390/app112110122Tipus de document
info:eu-repo/semantics/articleVersió de l'editorial
https://www.mdpi.com/2076-3417/11/21/10122Versió
info:eu-repo/semantics/publishedVersionParaules clau / Matèries
Resum
ZnO thin films with oxygen vacancies and doped with Al, Ga, and In (Zn1-xMxO1−y (x = 0.03)) have been successfully deposited on soda-lime glass substrates using a simple soft chemical method. The crystalline structure ... [+]
ZnO thin films with oxygen vacancies and doped with Al, Ga, and In (Zn1-xMxO1−y (x = 0.03)) have been successfully deposited on soda-lime glass substrates using a simple soft chemical method. The crystalline structure shows a single hexagonal phase of wurtzite with preferred crystal growth along the 002 plane. The surface morphology, characterized by SEM, revealed that the grain shape varies depending on the dopant agent used. Optical measurements displayed an increase in the bandgap values for doped films from 3.29 for ZnO to 3.35, 3.32, and 3.36 for Al, Ga, and In doped films, respectively, and an average transmittance superior to 90% in some cases (in the range between 400 and 800 nm). The electrical response of the films was evaluated with a four-point probe being 229.69, 385.71, and 146.94 Ω/sq for aluminium, gallium, and indium doped films, respectively. [-]
Publicat a
Applied Sciences, 2021, vol. 11, no 21Entitat finançadora
Ministerio de Economía y Competitividad (España)
Proyecto de investigación
ENE2017-87671-C3-3-RPID2020-116719RB-C43
Drets d'accés
info:eu-repo/semantics/openAccess
Apareix a les col.leccions
- QUIO_Articles [702]