Listar Departament: Enginyeria Mecànica i Construcció por fuente "Journal of Materials Processing Technology Volume 212, Issue 1, January 2012"
Mostrando ítems 1-1 de 1
-
Development of porous Ti6Al4V samples by microsphere sintering